Clarification of the optimum silica nanofiller amount for electrical treeing resistance

Z. Nawawi, M. A. B. Sidik, M. I. Jambak, C. L. G. Pavan Kumar, Aulia Aulia, M. H. Ahmad, A. A. Abd Jamil

Abstract


This paper aims to clarify the optimum amount of fumed silica (SiO2) nanofiller in resisting the initiation and propagation of electrical treeing in silicone rubber (SiR). Unlike other works, SiR/SiO2 nanocomposites containing seven different weight percentages of SiO2 nanofiller were prepared for this purpose. To achieve the objective, the electrical tree characteristics of the SiR/SiO2 nanocomposites were investigated by comparing the tree initiation voltage, tree breakdown time, tree propagation length and tree growth rate with its equivalent unfilled SiR. Moreover, the structural and morphological analyses were conducted on the SiR/SiO2 nanocomposite samples. The results showed that the SiR, when added with an appropriate amount of SiO2 nanofiller, could result in an improved electrical tree resistance. It implies that the 5 wt% of silica is the optimum amount to achieve the optimal electrical tree resistance such that above 5 wt%, the tree resistance performance has been abruptly reduced, subjected to the agglomeration issue.

Keywords


electrical treeing; nanocomposites; silica; silicone rubber;

Full Text:

PDF


DOI: http://doi.org/10.12928/telkomnika.v17i6.10605

Refbacks

  • There are currently no refbacks.


Creative Commons License
This work is licensed under a Creative Commons Attribution-ShareAlike 4.0 International License.

TELKOMNIKA Telecommunication, Computing, Electronics and Control
ISSN: 1693-6930, e-ISSN: 2302-9293
Universitas Ahmad Dahlan, 4th Campus
Jl. Ringroad Selatan, Kragilan, Tamanan, Banguntapan, Bantul, Yogyakarta, Indonesia 55191
Phone: +62 (274) 563515, 511830, 379418, 371120
Fax: +62 274 564604

View TELKOMNIKA Stats